TPU Pearlthane® 11T92EM

0

Technical Data Sheet

physical property Test ConditionTest MethodTest Result
densityASTM D7921.16 g/cm³
densityISO 27811.16 g/cm³
water content内部方法<0.10 %
hardnessTest ConditionTest MethodTest Result
Shore hardnessShore AASTMD224091
Mechanical propertiesTest ConditionTest MethodTest Result
Wear amountISO 464925.0 mm³
elastomerTest ConditionTest MethodTest Result
tensile strength ASTMD4128.00 MPa
tensile strength ASTMD41212.0 MPa
tensile strength YieldASTMD41235.0 MPa
elongationBreakASTMD412600 %
tear strengthASTM D624100 kN/m
tear strengthISO 34-1100 kN/m
compression setASTM D395B25 %
compression setASTM D395B43 %
Thermal performanceTest ConditionTest MethodTest Result
Glass Transition TemperatureISO 11357-2-38.0 °C
melting temperature内部方法180to190 °C
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.