physical property Test ConditionTest MethodTest Result
density0.980 g/cm³
Mooney viscosityASTM D164675 MU
bound acrylonitrile content内部方法33.0 %
stabilizerNon-staining
Soluble inMEK100 %
hardnessTest ConditionTest MethodTest Result
Shore hardnessASTM D224069
Shore hardnessASTM D224070
Shore hardnessASTM D224071
elastomerTest ConditionTest MethodTest Result
tensile strength ASTM D4129.12 MPa
tensile strength ASTM D41210.3 MPa
tensile strength ASTM D41210.9 MPa
tensile strength ASTM D41229.5 MPa
tensile strength ASTM D41229.0 MPa
elongationASTM D412650 %
elongationASTM D412590 %
elongationASTM D412560 %
tear strengthASTM D62462.8 kN/m
compression setASTM D39559 %
agingTest ConditionTest MethodTest Result
Change rate of hardness (Shore) in the airASTM D8652.0
Change rate of tensile strength in airASTM D4710.0 %
Change rate of tensile strength in airASTM D471-39 %
Change rate of ultimate elongation in airASTM D471-7.0 %
Change rate of ultimate elongation in airASTM D471-19 %
Change rate of hardness (Shore) in the airASTM D4710.0
Change rate of hardness (Shore) in the airASTM D471-6.0
volume changeASTM D4710.40 %
volume changeASTM D47114 %
Change rate of tensile strength in airASTM D8650.0 %
Change rate of ultimate elongation in airASTM D865-17 %
Thermal performanceTest ConditionTest MethodTest Result
Heat lossASTM D56880.30 %
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.