TPU Texalan® 2 Series 290A

0

Technical Data Sheet

physical property Test ConditionTest MethodTest Result
densityISO11831.19到1.23 g/cm³
hardnessTest ConditionTest MethodTest Result
Shore AISO86887到93
elastomerTest ConditionTest MethodTest Result
tear strengthISO34-1>110 kN/m
compression setISO815<45 %
elongationBreakISO37>500 %
Tensile stressISO37>8.50 MPa
Tensile stressISO37>15.0 MPa
Tensile stressYieldISO37>42.0 MPa
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.