Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|
Water absorption rate | Equilibrium | ISO 622 | 1.1 % |
density | | ISO 11832 | 1180 kg/m³ |
Melt volume flow rate | | ISO 11332 | 10.0 cm³/10min |
Water absorption rate | Saturation | ISO 622 | 2.3 % |
flammability | Test Condition | Test Method | Test Result |
---|
Burning Behav. | | ISO 12102 | HB |
Burning Behav.atthicknessh | | ISO 12102 | HB |
Mechanical properties | Test Condition | Test Method | Test Result |
---|
Tensile modulus | | ISO 527-22 | -- MPa |
tensile strength | Break | ISO 527-22 | -- MPa |
Tensile strain | Break | ISO 527-22 | -- % |
Tensile creep modulus | | ISO 899-12 | -- MPa |
Tensile creep modulus | | ISO 899-12 | -- MPa |
Electrical performance | Test Condition | Test Method | Test Result |
---|
Surface Resistivity | | IEC 600932 | -- ohms |
Volume resistivity | | IEC 600932 | -- ohms·m |
dielectric strength | | IEC 60243-12 | 35 kV/mm |
relative permittivity | | IEC 602502 | -- |
relative permittivity | | IEC 602502 | -- |
Dissipation Factor | | IEC 602502 | -- |
Dissipation Factor | | IEC 602502 | -- |
Compared to the Leakage Tracking Index (CTI) | | IEC 601122 | |
Thermal performance | Test Condition | Test Method | Test Result |
---|
melting temperature | | ISO 11357-32 | 255 °C |
Heat distortion temperature | | ISO 75-22 | 240 °C |
Heat distortion temperature | | ISO 75-22 | 220 °C |
vicat | | ISO 3062 | 160 °C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.