physical property Test ConditionTest MethodTest Result
Thickness0.0to2.3 µm
Supplementary InformationTest ConditionTest MethodTest Result
BackingMaterialPTFEFilm
CoreID7.62 cm
MaximumRollOD356 mm
Temperature of Use-101-260 °C
Width6.35to279 mm
filmTest ConditionTest MethodTest Result
tensile strength YieldASTM D88241.4 MPa
elongationBreakASTM D882330 %
Electrical performanceTest ConditionTest MethodTest Result
dielectric strengthASTM D14979 kV/mm
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.