Technical Data Sheet
physical property | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Melt Volume-Flow Rate (MVR) | 220°C/10.0kg | ISO1133 | 7.00 | cm3/10min |
Shrinkage rate | MD:23°C | ISO294-4 | 0.50到0.70 | % |
Mechanical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Rockwell hardness | R计秤,23°C | ISO2039-2 | 105 | |
Tensile modulus | 23°C | ISO527-2 | 1900 | Mpa |
tensile strength | 23°C | ISO527-2 | 49.0 | Mpa |
Bending modulus | 23°C | ISO178 | 2000 | Mpa |
Bending stress | 23°C | ISO178 | 73.0 | Mpa |
Thermal performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Hot deformation temperature | 1.8MPa,未退火 | ISO75-2/Af | 106 | °C |
Linear coefficient of thermal expansion | MD | ISO11359-2 | 8.5E-05 | cm/cm/°C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.