Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|
Shrinkage rate | | 东丽法 | 0.20 % |
Shrinkage rate | | 东丽法 | 0.70 % |
| | 东丽法 | 155 |
Basic performance | Test Condition | Test Method | Test Result |
---|
Water absorption rate | | ASTM D-570 | 0.02 % |
Mechanical properties | Test Condition | Test Method | Test Result |
---|
Impact Strength | | ASTM D-256 | 100 J/m |
Impact Strength | | ASTM D-256 | 30 KJ/m |
Curved elastic body | | ASTM D-790 | 14.7 GPa |
breaking strength | | ASTM D-732 | 75 |
tensile strength | | ASTM D-638 | 1.5 % |
Tensile strength | | ASTM D-638 | 140 Mpa |
Limit PV value | | 东丽法 | 815 KJ/m |
| | ASTM D-1894 | 0.25 |
bending strength | | ASTM D-790 | 200 Mpa |
hardness | | ASTM D-785 | 122 洛氏 |
| | ASTM D-1044 | 50 mg/1000回 |
Electrical performance | Test Condition | Test Method | Test Result |
---|
Inherent resistance of volume | | ASTM D-257 | 10 Ω.m |
Insulation breakdown voltage | | ASTM D-149 | 21 MV/m |
| | ASTM D-495 | 127 秒 |
Induced positive connection | | ASTM D-150 | 0.002 |
permittivity | | ASTM D-150 | 3.8 |
Thermal performance | Test Condition | Test Method | Test Result |
---|
| | ASTM D-696 | 2.2 |
| | ASTM D-696 | 3.3 |
| | DSC | 278 °C |
Heat distortion temperature | | ASTM D-648 | >260 °C |
combustibility | | UL-94 | V-0 |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.