Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|---|---|---|
density | ASTMD792 | 0.922 g/cm³ | |
ASTMD1238 | 1.0 g/10min |
optical performance | Test Condition | Test Method | Test Result |
---|---|---|---|
Haze ratio | ASTMD1003 | 9.5 % | |
gloss | ASTM2457 | 58 % | |
ASTM2457 | 85 % |
Other performance | Test Condition | Test Method | Test Result |
---|---|---|---|
temperature range | 155-185 °C | ||
Inflation ratio (BUR) | 2.0-3.0 | ||
material temperature | 175-185 °C | ||
Falling hammer impact | ASTMD1709 | 3.40 g/micron | |
falling weight impact test | ASTMD1709 | 170 g | |
Size of nozzle opening | 0.100 cm |
Mechanical properties | Test Condition | Test Method | Test Result |
---|---|---|---|
Secant modulus | ASTMD882 | 120 MPa | |
ASTMD882 | 130 MPa | ||
Tensile strength at break of thin film | ASTMD882 | 23.0 MPa | |
ASTMD882 | 21.0 MPa | ||
Elongation at break of thin film | ASTMD882 | 350 % | |
ASTMD882 | 620 % | ||
Elmendorf tear strength | ASTMD1922 | 6.20 g/micron | |
ASTMD1922 | 4.80 g/micron | ||
ASTMD1922 | 310 g | ||
ASTMD1922 | 240 g |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.