POM 100AL NC010 DUPONT USA
375
Form:Granules | Grade:Extrusion grade
Properties:
High rigidityHigh hardnessThermal stabilityhigh viscosityheat-resisting
Typical Applications:
Thin walled productsFitness equipment
Product Description
Certificates(1)
Datasheet
Product Description
| Typical Applications: | Thin walled products | Fitness equipment |
| Properties: | High rigidity | High hardness | Thermal stability | high viscosity | heat-resisting |
Certificates

Technical Data Sheet
| impact performance | Test Condition | Test Method | Test Result | Test Unit |
|---|---|---|---|---|
| Impact strength of cantilever beam gap | 23°C | ISO 180/1A | 8.0 | kJ/m² |
| Impact strength of simply supported beam without notch | 23°C | ISO 179/1eU | 250 | kJ/m² |
| -30°C | ISO 179/1eU | 170 | kJ/m² | |
| Charpy Notched Impact Strength | 23°C | ISO 179/1eA | 9.0 | kJ/m² |
| -30°C | ISO 179/1eA | 7.0 | kJ/m² | |
| flammability | Test Condition | Test Method | Test Result | Test Unit |
| Fogging-G-value | condensate | ISO 6452 | 1E-04 | g |
| FMVSS flammability | FMVSS302 | B | ||
| UL flame retardant rating | 1.5mm | IEC 60695-11-10,-20 | HB | |
| 0.8mm | IEC 60695-11-10,-20 | HB | ||
| 1.5mm | UL 94 | HB | ||
| 0.8mm | UL 94 | HB | ||
| Burning rate | 1.00mm | ISO 3795 | 26 | mm/min |
| mechanical properties | Test Condition | Test Method | Test Result | Test Unit |
| Tensile modulus | ISO 527-2 | 3000 | Mpa | |
| Bending modulus | ISO 178 | 2800 | Mpa | |
| tensile strength | Yield | ISO 527-2 | 70.0 | Mpa |
| Tensile strain | Yield | ISO 527-2 | 18 | % |
| Nominal tensile fracture strain | ISO 527-2 | 45 | % | |
| Tensile creep modulus | 1hr | ISO 899-1 | 2700 | Mpa |
| 1000hr | ISO 899-1 | 1500 | Mpa | |
| thermal performance | Test Condition | Test Method | Test Result | Test Unit |
| AnnealingTime-Optional | 30.0 | min/mm | ||
| AnnealingTemperature | 160 | °C | ||
| Linear coefficient of thermal expansion | TD | ISO 11359-2 | 1.1E-04 | cm/cm/°C |
| MD | ISO 11359-2 | 1.1E-04 | cm/cm/°C | |
| Melting temperature | ISO 11357-3 | 178 | °C | |
| Hot deformation temperature | 1.8MPa,Unannealed | ISO 75-2/A | 97.0 | °C |
| 0.45MPa,Unannealed | ISO 75-2/B | 163 | °C | |
| Physical properties | Test Condition | Test Method | Test Result | Test Unit |
| Shrinkage rate | MD | ISO 294-4 | 2.0 | % |
| TD | ISO 294-4 | 1.8 | % | |
| melt mass-flow rate | 190°C/2.16kg | ISO 1133 | 2.5 | g/10min |
| density | ISO 1183 | 1.40 | g/cm³ | |
| Supplementary Information | Test Condition | Test Method | Test Result | Test Unit |
| Emission | VDA275 | <8.00 | mg/kg |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.