Phenolic Resinoid 1382

0
  • Properties:
    Fillers
    glass fiber reinforced materials

Technical Data Sheet

physical property Test ConditionTest MethodTest Result
densityASTMD7921.88 g/cm³
Shrinkage rateASTMD9550.10 %
hardnessTest ConditionTest MethodTest Result
Rockwell hardnessM-ScaleASTMD785109
Rockwell hardnessASTMD78594
Mechanical propertiesTest ConditionTest MethodTest Result
tensile strengthYieldASTMD63879.3 MPa
Flexural modulusASTMD79016500 MPa
bending strengthYieldASTMD790114 MPa
compressive strengthASTMD695204 MPa
Impact resistanceTest ConditionTest MethodTest Result
Impact strength of cantilever beam gapASTMD256120 J/m
Electrical performanceTest ConditionTest MethodTest Result
dielectric strengthASTMD14913 kV/mm
Thermal performanceTest ConditionTest MethodTest Result
ASTMD648316 °C
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.