薄膜 | Test Condition | Test Method | Test Result |
---|---|---|---|
割线模量 | 1%正割,MD:31µm | ASTMD882 | >3000 MPa |
1%正割,TD:31µm | ASTMD882 | >1500 MPa | |
抗张强度 | MD:屈服,31µm | ASTMD882 | 125 MPa |
TD:屈服,31µm | ASTMD882 | 70.0 MPa | |
伸长率 | MD:断裂,31µm | ASTMD882 | 22 % |
TD:断裂,31µm | ASTMD882 | 70 % | |
密封强调 | 内部方法 | 2.2 N/mm | |
始封温度 | 31µm | 内部方法 | 100到160 °C |
透氧度(湿) | 23°C,31µm,0.0%RH | ASTMF1927 | 3.00 cm³/m²/24hr |
水蒸气透过性 | ASTME96 | 10 g/m²/24hr | |
薄膜厚度 | 内部方法 | 30.6 µm | |
用量 | 30.6µm | 内部方法 | 22.7 m²/kg |
光学性能 | Test Condition | Test Method | Test Result |
---|---|---|---|
光泽度 | 45°,30.6µm | ASTMD2457 | 105 |
雾度 | 30.6µm | ASTMD1003 | 4.0 % |
机械性能 | Test Condition | Test Method | Test Result |
---|---|---|---|
摩擦系数 | Itself - Dynamic | ASTMD1894 | 0.20 |
Itself - Static | ASTMD1894 | 0.25 |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.