Technical Data Sheet
thermosetting | Test Condition | Test Method | Test Result |
---|
Thermosetting components | Resin | | 按重量计算的混合比:100按容量计算的混合比:3.3 |
Thermosetting components | Hardener | | 按重量计算的混合比:18按容量计算的混合比:1.0 |
Thermosetting components | | | 180to240 min |
Thermosetting mixed viscosity | | ASTM D2393 | 2000to3000 cP |
physical property | Test Condition | Test Method | Test Result |
---|
density | | ASTM D792 | 1.45to1.50 g/cm³ |
hardness | Test Condition | Test Method | Test Result |
---|
Shore hardness | | ASTM D2240 | 83to87 |
Electrical performance | Test Condition | Test Method | Test Result |
---|
dielectric strength | | ASTM D149 | 21to23 kV/mm |
dielectric constant | | ASTM D2520 | 3.61to3.99 |
Dissipation Factor | | ASTM D150 | 0.014to0.015 |
Volume resistivity | | ASTM D257 | 1.9E+15到2.1E+15 ohms·cm |
Thermal performance | Test Condition | Test Method | Test Result |
---|
Glass Transition Temperature | | ASTME1356 | 76.0to84.0 °C |
Linear coefficient of thermal expansion | | ASTM D696 | 4.3E-5到4.7E-5 cm/cm/°C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.