63
Form:Granules | Grade:Injection grade
Properties:
Dimensional stabilityHigh mobilityHigh rigidityHeat agingHot water resistanceOil resistantFiller: Glass fiber reinf25%Filler by weight25%Filler by weight
Typical Applications:
Coil forming machineElectrical insulation componentsBearing ringEngineering accessoriesShellMechanical componentsMechanical accessoriesMachine/mechanical components
Product Description
Certificates(0)
Datasheet
Product Description
| Typical Applications: | Coil forming machine | Electrical insulation components | Bearing ring | Engineering accessories | Shell | Mechanical components | Mechanical accessories | Machine/mechanical components |
| Properties: | Dimensional stability | High mobility | High rigidity | Heat aging | Hot water resistance | Oil resistant | Filler: Glass fiber reinf | 25% | Filler by weight | 25% | Filler by weight |
Certificates
No Data...
Technical Data Sheet
| impact performance | Test Condition | Test Method | Test Result | Test Unit |
|---|---|---|---|---|
| Impact strength of cantilever beam gap | 23°C | ISO 180 | 7.1 | kJ/m² |
| -40°C | ISO 180 | 6.0 | kJ/m² | |
| Charpy Notched Impact Strength | 23°C | ISO 179 | 7.0 | kJ/m² |
| mechanical properties | Test Condition | Test Method | Test Result | Test Unit |
| Bending modulus | 23°C | ISO 178 | 7600 | Mpa |
| Tensile strain | Break,23°C | ISO 527-2 | 3.0 | % |
| tensile strength | Break,23°C | ISO 527-2 | 165 | Mpa |
| Tensile modulus | 23°C | ISO 527-2 | 8500 | Mpa |
| thermal performance | Test Condition | Test Method | Test Result | Test Unit |
| Melting temperature | ISO 3146 | 260 | °C | |
| Hot deformation temperature | 1.8MPa,Unannealed | ISO 75-2/A | 246 | °C |
| 0.45MPa,Unannealed | ISO 75-2/B | 260 | °C | |
| Physical properties | Test Condition | Test Method | Test Result | Test Unit |
| Water absorption rate | Equilibrium,23°C,50%RH | ISO 62 | 1.9 | % |
| Saturation,23°C | ISO 62 | 6.0 | % | |
| density | ISO 1183 | 1.32 | g/cm³ |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.