TPU-Ester EFRHATAN 90 CROSSPOLIMERI ITALY
Typical Applications:
Cable sheath wire and cable applications
Product Description
Certificates(0)
Datasheet
Product Description
| Typical Applications: | Cable sheath | wire and cable applications |
Certificates
No Data...
Technical Data Sheet
| flammability | Test Condition | Test Method | Test Result | Test Unit |
|---|---|---|---|---|
| Extreme Oxygen Index | ASTM D2863 | 22 | % | |
| elastomer | Test Condition | Test Method | Test Result | Test Unit |
| tear strength | DIN 53515 | 90 | kN/m | |
| mechanical properties | Test Condition | Test Method | Test Result | Test Unit |
| tensile strength | Yield | IEC 60811 | 49.0 | MPa |
| Tensile strain | Break | IEC 60811 | 550 | % |
| Wear resistance | DIN 53516 | 35.0 | mm³ | |
| thermal performance | Test Condition | Test Method | Test Result | Test Unit |
| ExerciseTemperature | 90 | °C | ||
| cold flexibility | ISO 458 | -22 | °C | |
| thermal stability | ISO R182 | >1 | hr | |
| Physical properties | Test Condition | Test Method | Test Result | Test Unit |
| density | ASTM D792 | 1.20 | g/cm³ | |
| hardness | Test Condition | Test Method | Test Result | Test Unit |
| Shore hardness | ShoreA | ASTM D2240 | 89 | |
| aging | Test Condition | Test Method | Test Result | Test Unit |
| Tensile stress change rate | 120°C,168hr,Break | UL 1581 | <30 | % |
| Change rate of tensile strength in air | 120°C,168hr | UL 1581 | <30 | % |
| 90°C,168hr,在ASTM#2油中 | UL 1581 | <30 | % | |
| 121°C,18hr,在ASTM#2油中 | UL 1581 | <30 | % | |
| Tensile stress change rate | 90°C,168hr,在ASTM#2油中,Break | UL 1581 | <30 | % |
| 121°C,18hr,在ASTM#2油中,Break | UL 1581 | <30 | % |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.