PA6 PA6-FG430
0
- Properties:30% glass fiber reinforced flame retardant gradehigh strength
- Usages:Mainly used in various internal terminal blockstransformer spoolsconnectorsswitch socket componentsfuse boxesetc. with flame retardant requirements
Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|---|---|---|
Shrinkage rate | ASTM D955 | 0.6 % | |
density | ASTM D792 | 1.6 g/cm | |
Water absorption rate | ASTM D570 | 1.4-1.8 % | |
Shrinkage rate | ASTM D955 | 0.3 % |
Mechanical properties | Test Condition | Test Method | Test Result |
---|---|---|---|
tensile strength | ASTM D638 | 133 MPa | |
elongation | Break | ASTM D638 | 2.8 % |
bending strength | ASTM D790 | 190 MPa | |
Flexural modulus | ASTM D790 | 8100 MPa | |
Impact strength of cantilever beam gap | ASTM D256 | 12 KJ/m |
Other performance | Test Condition | Test Method | Test Result |
---|---|---|---|
UL flame retardant rating | UL94 | V-0 级 |
Electrical performance | Test Condition | Test Method | Test Result |
---|---|---|---|
Volume resistivity | IEC 60093 | 10 Ω·m | |
Compared to the Leakage Tracking Index (CTI) | UL-746A | 伏 |
Thermal performance | Test Condition | Test Method | Test Result |
---|---|---|---|
Heat distortion temperature | ASTM D648 | 205 ℃ | |
ASTM D648 | 220 ℃ | ||
melting temperature | ASTM D789 | 220 ℃ |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.