physical property | Test Condition | Test Method | Test Result |
---|
density | | ASTM D792 | 1.07 g/cm³ |
density | | ISO 2781 | 1.07 g/cm³ |
water content | | 内部方法 | <0.10 % |
hardness | Test Condition | Test Method | Test Result |
---|
Shore hardness | Shore A | ASTMD2240 | 72 |
Mechanical properties | Test Condition | Test Method | Test Result |
---|
Wear amount | | ISO 4649 | 25.0 mm³ |
elastomer | Test Condition | Test Method | Test Result |
---|
tensile strength | | ASTMD412 | 3.00 MPa |
tensile strength | | ASTMD412 | 5.00 MPa |
tensile strength | Yield | ASTMD412 | 30.0 MPa |
elongation | Break | ASTMD412 | 710 % |
tear strength | | ASTM D624 | 65.0 kN/m |
tear strength | | ISO 34-1 | 65 kN/m |
compression set | | ASTM D395B | 30 % |
compression set | | ASTM D395B | 60 % |
Thermal performance | Test Condition | Test Method | Test Result |
---|
Glass Transition Temperature | | ISO 11357-2 | -53.0 °C |
melting temperature | | 内部方法 | 168to178 °C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.