Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|
density | | ISO1183 | 0.940 g/cm³ |
melt mass-flow rate | | ISO1133 | 20 g/10min |
Vinyl acetate content | | | 18.0 wt% |
hardness | Test Condition | Test Method | Test Result |
---|
| Shore A | ISO868 | 84 |
| | ISO868 | 30 |
Supplementary Information | Test Condition | Test Method | Test Result |
---|
ProcessingTemperature | | | 100到150 °C |
Mechanical properties | Test Condition | Test Method | Test Result |
---|
Tensile stress | Break | ISO527-2/1BA | 11.0 MPa |
Tensile stress | | ISO527-2/1BA | 3.90 MPa |
Tensile strain | Break | ISO527-2/1BA | >600 % |
Thermal performance | Test Condition | Test Method | Test Result |
---|
vicat | | ISO306/A | 50.0 °C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.