PA46 TW275F6 DSM HOLAND
35
Form:Granules | Grade:Injection grade
Properties:
wear resistantThermal stability
Typical Applications:
Automotive ApplicationsHome appliance components
Product Description
Certificates(0)
Datasheet
Product Description
| Typical Applications: | Automotive Applications | Home appliance components |
| Properties: | wear resistant | Thermal stability |
Certificates
No Data...
Technical Data Sheet
| impact performance | Test Condition | Test Method | Test Result | Test Unit |
|---|---|---|---|---|
| Impact strength of simply supported beam without notch | -30°C | ISO 179/1eU | 60 | kJ/m² |
| 23°C | ISO 179/1eU | 75 | kJ/m² | |
| mechanical properties | Test Condition | Test Method | Test Result | Test Unit |
| tensile strength | Break | ISO 527-2 | 205 | Mpa |
| Break, 120°C | ISO 527-2 | 110 | Mpa | |
| Break, 160°C | ISO 527-2 | 100 | Mpa | |
| Break, 180°C | ISO 527-2 | 95.0 | Mpa | |
| Break, 200°C | ISO 527-2 | 90.0 | Mpa | |
| Tensile strain | Break | ISO 527-2 | 3.5 | % |
| Break, 120°C | ISO 527-2 | 8.4 | % | |
| Break, 160°C | ISO 527-2 | 8.9 | % | |
| Break, 180°C | ISO 527-2 | 9.1 | % | |
| Break, 200°C | ISO 527-2 | 9.4 | % | |
| Bending modulus | ISO 178 | 9000 | Mpa | |
| thermal performance | Test Condition | Test Method | Test Result | Test Unit |
| Hot deformation temperature | 0.45 MPa, Unannealed | ISO 75-2/B | 290 | °C |
| 1.8 MPa, Unannealed | ISO 75-2/A | 285 | °C | |
| Melting temperature | ISO 11357-3 | 295 | °C | |
| Linear coefficient of thermal expansion | Flow | ISO 11359-2 | 2.5E-5 | cm/cm/°C |
| Across Flow | ISO 11359-2 | 6.0E-5 | cm/cm/°C | |
| Physical properties | Test Condition | Test Method | Test Result | Test Unit |
| Shrinkage rate | 横向Flow | ISO 294-4 | 1.3 | % |
| Flow | ISO 294-4 | 0.50 | % | |
| Water absorption rate | Equilibrium, 23°C, 50% RH | ISO 62 | 2.5 | % |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.