EHMWPE BAAF UHMW-PE 4000 NC

0

Technical Data Sheet

physical property Test ConditionTest MethodTest Result
density内部方法0.935到0.940 g/cm³
Apparent density内部方法>0.35 g/cm³
molecular weight内部方法>4000000
Volatile compounds内部方法<0.15 wt%
Particle size内部方法>98.0 %
Mechanical propertiesTest ConditionTest MethodTest Result
Tensile stressBreak内部方法>30.0 MPa
Tensile strainBreak内部方法200 %
Impact resistanceTest ConditionTest MethodTest Result
Impact strength of cantilever beam gap内部方法>70 kJ/m²
内部方法无断裂
Thermal performanceTest ConditionTest MethodTest Result
内部方法>80.0 °C
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.