Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|---|---|---|
water content | 7.4 wt% | ||
solubility | 27.0 sec | ||
10.0 sec | |||
155.0 sec | |||
93.0 sec |
film | Test Condition | Test Method | Test Result |
---|---|---|---|
usage | ASTM D4321 | 15.6 m²/kg | |
Secant modulus | ASTMD882 | 19.3 MPa | |
tensile strength | ASTM D882 | 33.8 MPa | |
ASTM D882 | 45.5 MPa | ||
ISO 527-3 | 33.8 MPa | ||
ISO 527-3 | 45.5 MPa | ||
elongation | ASTMD882 | 290 % | |
ASTMD882 | 280 % | ||
Dart impact | ASTMD1709 | 960 g | |
Elmendorf tear strength | ASTM D1922 | 1300 g | |
Secant modulus | ASTMD882 | 73.8 MPa | |
Elmendorf tear strength | ISO 6383-2 | 0.13 N | |
ISO 6383-2 | 0.13 N | ||
film thickness | 50 µm | ||
20µmto60µm | |||
Secant modulus | ASTMD882 | 68.3 MPa | |
ASTMD882 | 17.9 MPa | ||
Elmendorf tear strength | ASTM D1922 | 1300 g |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.