HDPE 3080

27
  • Properties:
    High toughness
    packing
  • Usages:
    Bag
    chip

Technical Data Sheet

Basic performanceTest ConditionTest MethodTest Result
Dart impact0.952 g/cm
Mechanical propertiesTest ConditionTest MethodTest Result
tensile strength 250 kg/cm
tensile strength 380 kg/cm
elongation at breakASTM D638/ISO 527800 %
tensile strength ASTM D638/ISO 527380 kg/cm²(MPa)[Lb/in²]
Rockwell hardnessASTM D78564
Other performanceTest ConditionTest MethodTest Result
Shore hardness64
melt mass-flow rate0.08 g/10min
elongation800 %
Physical propertiesTest ConditionTest MethodTest Result
densityASTM D792/ISO 11830.952
melt mass-flow rateASTM D1238/ISO 11330.08 g/10min
Thermal performanceTest ConditionTest MethodTest Result
vicat125 °C
melting temperature132 °C
melting temperature132 ℃(℉)
vicatASTM D1525/ISO R306125 ℃(℉)
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.