Technical Data Sheet
thermosetting | Test Condition | Test Method | Test Result |
---|
| | | 按重量计算的混合比:100按容量计算的混合比:1.0 |
| | | 按重量计算的混合比:120按容量计算的混合比:1.0 |
| | | 0.0到2.0 min |
Thermosetting mixed viscosity | | ASTMD2393 | 500到800 cP |
physical property | Test Condition | Test Method | Test Result |
---|
density | | ASTMD792 | 1.04到1.06 g/cm³ |
hardness | Test Condition | Test Method | Test Result |
---|
| | ASTMD2240 | 60到65 |
Electrical performance | Test Condition | Test Method | Test Result |
---|
Volume resistivity | | ASTMD257 | 1.0E+14到4.0E+14 ohms·cm |
dielectric strength | | ASTMD149 | 20到22 kV/mm |
dielectric constant | | ASTMD2520 | 3.10到3.50 |
Dissipation Factor | | ASTMD150 | 0.050到0.070 |
Thermal performance | Test Condition | Test Method | Test Result |
---|
Glass Transition Temperature | | ASTME1356 | -15.0到-12.0 °C |
| | ASTMD696 | 2.3E-4到2.8E-4 cm/cm/°C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.