HMW-HDPE HDPE PE80

0

Technical Data Sheet

physical property Test ConditionTest MethodTest Result
melt mass-flow rateASTMD12388.5 g/10min
Resistance to environmental stress crackingASTMD1693A500 hr
ESCR - NCTLASTMF213616.7 day
melt mass-flow rateASTMD12380.040 g/10min
densityASTMD7920.947 g/cm³
Mechanical propertiesTest ConditionTest MethodTest Result
tensile strengthYieldASTMD63824.8 MPa
elongationBreakASTMD638600 %
Impact resistanceTest ConditionTest MethodTest Result
Tensile impact strengthASTMD1822242 kJ/m²
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.