PA66 A3WG6-BK BASF GERMANY
302
Form:Granules | Grade:Enhanced level
Properties:
High rigidityOil resistantdimensional stability heat-resisting
Typical Applications:
machineMechanical componentscontainerProfileAutomotive sectorShell
Product Description
Certificates(1)
Datasheet
Product Description
| Typical Applications: | machine | Mechanical components | container | Profile | Automotive sector | Shell |
| Properties: | High rigidity | Oil resistant | dimensional stability | heat-resisting |
Certificates

Technical Data Sheet
| other | Test Condition | Test Method | Test Result | Test Unit |
|---|---|---|---|---|
| UL flame retardant rating | 1.50 mm | UL 94 | HB | |
| mechanical properties | Test Condition | Test Method | Test Result | Test Unit |
| Impact strength of cantilever beam gap | 23℃ | ISO 180 | 8.5 | kJ/m² |
| Bending modulus | 23℃ | ISO 178 | 8730 | Mpa |
| Tensile strain | Break | ISO 527-22 | 2.6 | % |
| tensile strength | Break | ISO 527-22 | 179 | Mpa |
| thermal performance | Test Condition | Test Method | Test Result | Test Unit |
| Hot deformation temperature | 1.8 MPa | ISO 75-22 | 250 | °C |
| Melting temperature | DSC | ASTM D3418 | 260 | °C |
| Physical properties | Test Condition | Test Method | Test Result | Test Unit |
| Water absorption rate | Equilibrium | ISO 622 | 1.7 | % |
| Equilibrium, 50% RH | ASTM D570 | 1.7 | % | |
| Saturation | ASTM D570 | 5.5 | % | |
| Shrinkage rate | MD | ASTM D955 | 0.30 | % |
| density | -- | ISO 11832 | 1360 | kg/m3 |
| -- | ASTM D792 | 1.36 | g/cm³ |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.