PA6 B3EG3 BASF GERMANY
332
Form:Granules | Grade:Injection grade
Properties:
Oil resistantHigh impact resistanceFiller: Glass fiber reinf15%Filler by weight
Typical Applications:
Automotive sectorwheelShellApplication in the automotive fieldwheelShell
Product Description
Certificates(1)
Datasheet
Product Description
| Typical Applications: | Automotive sector | wheel | Shell | Application in the automotive field | wheel | Shell |
| Properties: | Oil resistant | High impact resistance | Filler: Glass fiber reinf | 15% | Filler by weight |
Certificates

Technical Data Sheet
| impact performance | Test Condition | Test Method | Test Result | Test Unit |
|---|---|---|---|---|
| Impact strength of cantilever beam gap | 23°C | ISO 180 | 5.0 | kJ/m² |
| -30°C | ISO 180 | 4.5 | kJ/m² | |
| Charpy Notched Impact Strength | 23°C | ISO 179 | 5.0 | kJ/m² |
| mechanical properties | Test Condition | Test Method | Test Result | Test Unit |
| Bending modulus | 23°C | ISO 178 | 5300 | Mpa |
| Tensile strain | Break,23°C | ISO 527-2 | 2.5 | % |
| tensile strength | Break,23°C | ISO 527-2 | 115 | Mpa |
| Tensile modulus | 23°C | ISO 527-2 | 6060 | Mpa |
| thermal performance | Test Condition | Test Method | Test Result | Test Unit |
| Melting temperature | ISO 3146 | 220 | °C | |
| Hot deformation temperature | 1.8MPa,Unannealed | ISO 75-2/A | 200 | °C |
| 0.45MPa,Unannealed | ISO 75-2/B | 217 | °C | |
| Physical properties | Test Condition | Test Method | Test Result | Test Unit |
| Water absorption rate | Equilibrium,23°C,50%RH | ISO 62 | 2.3 | % |
| Saturation,23°C | ISO 62 | 7.7 | % | |
| density | ISO 1183 | 1.23 | g/cm³ | |
| Electrical performance | Test Condition | Test Method | Test Result | Test Unit |
| Dissipation factor | 1MHz | IEC 60250 | 0.025 | |
| 100Hz | IEC 60250 | 0.025 | ||
| Dielectric constant | 1MHz | IEC 60250 | 3.80 | |
| Volume resistivity | IEC 60093 | 1E+13 | ohms·cm |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.