EVA Escorene™ Ultra UL 7765
34
- Properties:High softness and softnesLow temperature toughnessFiller: ExxonMobil Chemic
- Usages:Wire and cablesealantadhesiveHot melt adhesive
Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|---|---|---|
melt mass-flow rate | ASTM D1238 | 2.3 g/10min | |
density | ASTM D1505 | 0.950 g/cm³ | |
Vinyl acetate content | ExxonMobilMethod | 26.2 wt% |
hardness | Test Condition | Test Method | Test Result |
---|---|---|---|
Shore hardness | Shore A,15sec | ASTM D2240 | 84 |
Shore D,15sec | ASTM D2240 | 29 |
Mechanical properties | Test Condition | Test Method | Test Result |
---|---|---|---|
elongation | Break | ASTM D638 | >800 % |
Flexural modulus | ASTM D790 | 33 Mpa |
Impact resistance | Test Condition | Test Method | Test Result |
---|---|---|---|
Dart impact | ASTM D3763 | 24.4 J | |
ASTM D3763 | 21.7 J |
Thermal performance | Test Condition | Test Method | Test Result |
---|---|---|---|
vicat | ASTM D1525 | 67 °C | |
melting temperature | Break | 75 ℃ |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.