Test Condition | Test Method | Test Result | |
---|---|---|---|
density | 0.924 g/cm³ | ||
melt mass-flow rate | ASTM D1238 | 2.0 g/10min | |
Vinyl acetate content | 5.5 wt% | ||
Secant modulus | ASTM D882 | 127 MPa | |
ASTM D882 | 146 MPa | ||
elongation | ASTM D882 | 590 % | |
Dart impact | ASTM D1709 | 170 g | |
Elmendorf tear strength | ASTM D1922 | 160 g | |
ASTM D1922 | 75 g | ||
melting temperature | 102 °C | ||
gloss | ASTM D2457 | 74 | |
Haze ratio | ASTM D1003 | 4.0 % | |
tensile strength | ASTM D882 | 25.1 MPa | |
ASTM D882 | 23.9 MPa | ||
elongation | ASTM D882 | 190 % |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.