Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|
density | | ISO1183 | 1.35 g/cm³ |
Melt volume flow rate | | ISO1133 | 7.00 cm³/10min |
Mechanical properties | Test Condition | Test Method | Test Result |
---|
Tensile stress | | ISO527-2 | 45.0 MPa |
Tensile strain | | ISO527-2 | 16 % |
Nominal tensile fracture strain | | ISO527-2 | 40 % |
Tensile creep modulus | | ISO899-1 | 500 MPa |
Tensile modulus | | ISO527-2 | 1500 MPa |
Impact resistance | Test Condition | Test Method | Test Result |
---|
Charpy Notched Impact Strength | | ISO179 | 8.0 kJ/m² |
Charpy Notched Impact Strength | | ISO179 | 15 kJ/m² |
Impact strength of simply supported beam without notch | | ISO179 | 270 kJ/m² |
Impact strength of simply supported beam without notch | | ISO179 | NoBreak |
Electrical performance | Test Condition | Test Method | Test Result |
---|
Surface Resistivity | | IEC60093 | 1E+14 ohms |
Volume resistivity | | IEC60093 | 1E+13 ohms·cm |
dielectric constant | | IEC60250 | 4.20 |
Dissipation Factor | | IEC60250 | 0.017 |
CTI | | IEC60112 | 600 V |
Thermal performance | Test Condition | Test Method | Test Result |
---|
| | ISO3146 | 167 °C |
| | | 1.3E-04 cm/cm/°C |
Heat distortion temperature | | ISO75-2/A | 80.0 °C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.