TPE 2165 Ningxia Chemical
0
- Properties:Injection molding reference process: temperature at the rear of the barrel 140-160 ℃ holding pressure 30-120MPa temperature at the middle of the barrel 150-170 ℃ mold temperature 20-50 ℃ temperature at the front of the barrel 160-180 ℃ holding time 15-75S nozzle temperature 170-190 ℃ screw speed 20-100r min injection pressure 40-150MPa injection speed medium fast back pressure
Technical Data Sheet
| Other performance | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Constant tensile strength retention rate | 100% | 125 % | |
| Volume change of fuel B | 室温×96h | -12 % | |
| Permanent compression deformation | 37 % | ||
| Change rate of tensile strength in air | 112 % | ||
| Elongation at Break | 97 % |
| Basic Performance | Test Condition | Test Method | Test Result |
|---|---|---|---|
| density | 1.18 |
| mechanical properties | Test Condition | Test Method | Test Result |
|---|---|---|---|
| tear strength | 32.0 kN/m | ||
| Shore hardness | 65 A | ||
| tensile strength | 11.0 MPa | ||
| Elongation at Break | 430 % | ||
| Tensile stress | 100% | 3.5 MPa |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.