physical property | Test Condition | Test Method | Test Result |
---|
density | | ASTM D-792 | 1.04 g/cm |
processability | Test Condition | Test Method | Test Result |
---|
Shrinkage rate of mold | | ASTM D-955 | 0.4-0.7 % |
Processing melting temperature | | | 200-240 ℃ |
Basic performance | Test Condition | Test Method | Test Result |
---|
melt mass-flow rate | | ASTM D-1238 | 4 g/10min |
Mechanical properties | Test Condition | Test Method | Test Result |
---|
IZOD impact strength | | ASTM D-256 | 10 kg.cm/cm |
Rockwell hardness | | ASTM D-785 | R-76 |
elongation | Break | ASTM D-638 | 55 % |
Rubbing modulus | | ASTM D-790 | 20000 kg/cm |
tensile yield strength | | ASTM D-638 | 260 kg/cm |
| | ASTM D-790 | 45 kg/cm |
Thermal performance | Test Condition | Test Method | Test Result |
---|
drying temperature | | | 70 ℃ |
flammability | | UL-94 | HB |
| | ASTM D-648 | 73 ℃ |
vicat | | ASTM D-1525 | 89 ℃ |
vicat | | ASTM D-1525 | 97 ℃ |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.