PS Electroblend® HIPS-4900

0
  • Usages:
    Applications in the automotive
    electrical
    and electronic fields

Technical Data Sheet

physical property Test ConditionTest MethodTest Result
densityASTMD7921.00 g/cm³
Shrinkage rateASTMD9550.40到0.70 %
flammabilityTest ConditionTest MethodTest Result
UL flame retardant ratingUL94HB
Mechanical propertiesTest ConditionTest MethodTest Result
tensile strengthASTMD63828.0 MPa
elongationBreakASTMD63873 %
Flexural modulusASTMD7902520 MPa
bending strengthASTMD79044.0 MPa
Impact resistanceTest ConditionTest MethodTest Result
Impact strength of cantilever beam gapASTMD256140 J/m
Electrical performanceTest ConditionTest MethodTest Result
Surface ResistivityASTMD2571.0E+6到1.0E+10 ohms
Thermal performanceTest ConditionTest MethodTest Result
ASTMD64880.0 °C
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.