PP Tecnoprene® A60K6 NAT001 SO.F.TER ITALY
Properties:
Filler glass fiber reinforced material 30% filler by weight
Product Description
Certificates(0)
Datasheet
Product Description
| Properties: | Filler | glass fiber reinforced material | 30% | filler by weight |
Certificates
No Data...
Technical Data Sheet
| impact performance | Test Condition | Test Method | Test Result | Test Unit |
|---|---|---|---|---|
| Charpy Notched Impact Strength | 23°C | ISO 179/1eA | 12 | kJ/m² |
| Impact strength of simply supported beam without notch | 23°C | ISO 179/1eU | 40 | kJ/m² |
| Impact strength of cantilever beam gap | -20°C | ASTM D256 | 110 | J/m |
| 23°C | ASTM D256 | 130 | J/m | |
| flammability | Test Condition | Test Method | Test Result | Test Unit |
| UL flame retardant rating | 3.2mm | UL 94 | HB | |
| mechanical properties | Test Condition | Test Method | Test Result | Test Unit |
| tensile strength | Break | ASTM D638 | 90.0 | MPa |
| Bending modulus | ASTM D790 | 6200 | MPa | |
| bending strength | ASTM D790 | 135 | MPa | |
| thermal performance | Test Condition | Test Method | Test Result | Test Unit |
| Hot deformation temperature | 1.8MPa,Unannealed | ASTM D648 | 150 | °C |
| Vicat softening temperature | ASTM D15253 | 138 | °C | |
| Linear coefficient of thermal expansion | MD | ASTM D696 | 5.5E-05 | cm/cm/°C |
| Physical properties | Test Condition | Test Method | Test Result | Test Unit |
| Shrinkage rate | Internal Method | 0.50 | % | |
| Water absorption rate | 23°C,24hr | ASTM D570 | 0.020 | % |
| ash content | Internal Method | 30 | % | |
| density | ASTM D792 | 1.12 | g/cm³ | |
| melt mass-flow rate | 230°C/2.16kg | ASTM D1238 | 3.0 | g/10min |
| Electrical performance | Test Condition | Test Method | Test Result | Test Unit |
| Dielectric constant | 1kHz | ASTM D150 | 2.60 | |
| Compared to the anti leakage trace index | IEC 60112 | PLC 0 | ||
| Surface resistivity | ASTM D257 | 1E+15 | ohms |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.