Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|
Shrinkage rate | | | -1.7 % |
Shrinkage rate | | | -1.1 % |
density | | | 0.0500 g/cm³ |
Thickness | | | 1.50 mm |
hardness | Test Condition | Test Method | Test Result |
---|
Compressive Hardness | | | 0.0990 MPa |
Supplementary Information | Test Condition | Test Method | Test Result |
---|
GelFraction | | | 35 % |
ThermoformingRatio-H/D | | | 0.720 |
Mechanical properties | Test Condition | Test Method | Test Result |
---|
elongation | | | 300 % |
elongation | | | 240 % |
elastomer | Test Condition | Test Method | Test Result |
---|
tensile strength | | | 0.756 MPa |
tensile strength | | | 1.09 MPa |
tear strength | Across Flow | | 7.00 kN/m |
tear strength | | | 4.90 kN/m |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.