Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|
Shrinkage rate | | ISO294-4 | 1.5 % |
density | | ISO1183 | 0.890 g/cm³ |
Melt volume flow rate | | ISO1133 | 6.00 cm³/10min |
SpiralFlow | | 内部方法 | 28.0 cm |
hardness | Test Condition | Test Method | Test Result |
---|
| | ISO868 | 33 |
Mechanical properties | Test Condition | Test Method | Test Result |
---|
Tensile stress | Break | ISO527-2/5A/500 | 13.0 MPa |
Tensile stress | | ISO527-2/5A/500 | 23.6 MPa |
Tensile stress | | ISO527-2/5A/500 | 3.70 MPa |
Tensile strain | Break | ISO527-2/5A/500 | 180 % |
Tensile strain | | ISO527-2/5A/500 | 73 % |
Tensile strain | | ISO527-2/5A/500 | 180 % |
Flexural modulus | | ISO178 | 240 MPa |
Flexural modulus | | ISO178 | 69.0 MPa |
Impact resistance | Test Condition | Test Method | Test Result |
---|
NotchedIzodImpactStrength | | ISO180 | 75 kJ/m² |
elastomer | Test Condition | Test Method | Test Result |
---|
tear strength | | ISO34-1 | 76 kN/m |
tear strength | | ISO34-1 | 150 kN/m |
tear strength | | ISO34-1 | 47 kN/m |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.