plas
Log In

Rubber RTV-2 XP-643 Silicones, Inc.

0

Technical Data Sheet

Cured PropertiesTest ConditionTest MethodTest Result
tear strength22.8to26.3 kN/m
elongationBreak680to730 %
tensile strength4.65to5.34 MPa
Shore hardnessShoreA36to44
Uncured PropertiesTest ConditionTest MethodTest Result
ColorPot Life60 min
Color--3OffWhite
Color--2Blue
thermosettingTest ConditionTest MethodTest Result
Thermosetting mixed viscosityASTM D239325000 cP
shelf-life26 wk
Physical propertiesTest ConditionTest MethodTest Result
density1.13 g/cm³
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.