Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|---|---|---|
density | ASTMD792 | 1.01 g/cm³ | |
Biomass content | <30.0 |
film | Test Condition | Test Method | Test Result |
---|---|---|---|
tensile strength | ASTMD882 | 53.0 MPa | |
ASTMD882 | 30.9 MPa | ||
elongation | ASTMD882 | 480 % | |
ASTMD882 | 680 % | ||
Falling hammer impact | ASTMD1709 | 450 g | |
Elmondov tear strength | ASTMD1922 | 320 g | |
ASTMD1922 | 620 g | ||
Oxygen transmission rate | ASTMD3985 | 7100 cm³/m²/24hr | |
Secant modulus | ASTMD882 | 193 MPa | |
ASTMD882 | 288 MPa | ||
Water vapor permeability | 内部方法 | 9.0 g/m²/24hr |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.