PPO(PPE)+PS Generic PPE+PS+Nylon - Mineral Generic
Properties:
Filler mineral filler
Product Description
Certificates(0)
Datasheet
Product Description
| Properties: | Filler | mineral filler |
Certificates
No Data...
Technical Data Sheet
| impact performance | Test Condition | Test Method | Test Result | Test Unit |
|---|---|---|---|---|
| Charpy Notched Impact Strength | 23°C | ISO 179 | 3.5to4.0 | kJ/m² |
| Impact strength of cantilever beam gap | 23°C | ISO 180 | 4.0to4.5 | kJ/m² |
| mechanical properties | Test Condition | Test Method | Test Result | Test Unit |
| Tensile modulus | 23°C | ISO 527-2 | 4200to4790 | MPa |
| tensile strength | Break,23°C | ISO 527-2 | 60.0to65.0 | MPa |
| Tensile strain | Break,23°C | ISO 527-2 | 4.0to7.0 | % |
| Bending modulus | 23°C | ISO 178 | 4000to4440 | MPa |
| bending strength | 23°C | ISO 178 | 105to110 | MPa |
| thermal performance | Test Condition | Test Method | Test Result | Test Unit |
| Hot deformation temperature | 0.45MPa,Unannealed | ISO 75-2/B | 184to205 | °C |
| Vicat softening temperature | ISO 306 | 185to200 | °C | |
| Linear coefficient of thermal expansion | MD | ISO 11359-2 | 5.0E-5到6.0E-5 | cm/cm/°C |
| TD | ISO 11359-2 | 6.5E-05 | cm/cm/°C | |
| Physical properties | Test Condition | Test Method | Test Result | Test Unit |
| density | 23°C | ISO 1183 | 1.20to1.25 | g/cm³ |
| Shrinkage rate | MD:23°C | ASTM D955 | 0.80to1.1 | % |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.