PBT TEKASTER™ F10G30

0
  • Properties:
    Filler
    glass fiber reinforced material
    30%
    filler by weight

Technical Data Sheet

physical property Test ConditionTest MethodTest Result
Shrinkage rateASTM D9550.30to0.90 %
densityASTM D7921.52 g/cm³
flammabilityTest ConditionTest MethodTest Result
UL flame retardant ratingUL 94HB
Mechanical propertiesTest ConditionTest MethodTest Result
tensile strength BreakASTM D638118 MPa
elongationBreakASTM D6383.0 %
Flexural modulusASTM D7907750 MPa
bending strengthASTM D790181 MPa
Impact resistanceTest ConditionTest MethodTest Result
Impact strength of cantilever beam gapASTM D25678 J/m
Thermal performanceTest ConditionTest MethodTest Result
Heat distortion temperatureASTM D648210 °C
Heat distortion temperatureASTM D648215 °C
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.