impact performanceTest ConditionTest MethodTest ResultTest Unit
Suspended wall beam without notch impact strength23°CISO 180/1U50kJ/m²
Suspended wall beam without notch impact strength-30°CISO 180/1U40kJ/m²
Charpy Notched Impact Strength-30°CISO 179/1eA6.0kJ/m²
Charpy Notched Impact Strength23°CISO 179/1eA7.0kJ/m²
Impact strength of simply supported beam without notch-30°CISO 179/1eU45kJ/m²
Impact strength of simply supported beam without notch23°CISO 179/1eU55kJ/m²
Impact strength of cantilever beam gap-40°CISO 180/1A6.0kJ/m²
Impact strength of cantilever beam gap-30°CISO 180/1A7.0kJ/m²
Impact strength of cantilever beam gap-20°CISO 180/1A7.0kJ/m²
Impact strength of cantilever beam gap23°CISO 180/1A8.0kJ/m²
flammabilityTest ConditionTest MethodTest ResultTest Unit
UL flame retardant rating0.75mmUL 94HB
Burning wire flammability index2.0mmIEC 60695-2-12650°C
Extreme Oxygen IndexISO 4589-224%
mechanical propertiesTest ConditionTest MethodTest ResultTest Unit
Tensile modulusISO 527-2/16500MPa
tensile strengthBreakISO 527-2/5145MPa
Tensile strainBreakISO 527-2/53.8%
Bending modulusISO 1785800MPa
Taber abraser1000Cycles,1000g,CS-17WheelInternal Method20.0mg
bending strengthISO 178200MPa
thermal performanceTest ConditionTest MethodTest ResultTest Unit
Hot deformation temperature0.45MPa,Unannealed,100mmSpanISO 75-2/Be216°C
Hot deformation temperature1.8MPa,Unannealed,100mmSpanISO 75-2/Ae198°C
Vicat softening temperature--ISO 306/B50208°C
Vicat softening temperature--ISO 306/B120206°C
Ball Pressure Test125°CIEC 60695-10-2通过
Linear coefficient of thermal expansionMD:23to60°CISO 11359-23.5E-05cm/cm/°C
Linear coefficient of thermal expansionTD:23to60°CISO 11359-29.5E-05cm/cm/°C
thermal conductivityISO 83020.33W/m/K
Physical propertiesTest ConditionTest MethodTest ResultTest Unit
densityISO 11831.27g/cm³
Shrinkage rateMDInternal Method0.30to0.60%
Water absorption rateSaturation,23°CISO 626.8%
Water absorption rateEquilibrium,23°C,50%RHISO 621.4%
Electrical performanceTest ConditionTest MethodTest ResultTest Unit
Volume resistivityIEC 60093>1.0E+16ohms·cm
Dielectric strength3.20mm,in OilIEC 60243-120kV/mm
Relative permittivity50HzIEC 602503.60
Relative permittivity60HzIEC 602503.60
Relative permittivity1MHzIEC 602503.40
Dissipation factor50HzIEC 602506.1E-03
Dissipation factor60HzIEC 602506.1E-03
Dissipation factor1MHzIEC 602500.016
Compared to the anti leakage trace index--IEC 60112PLC 1
Compared to the anti leakage trace indexSolutionBIEC 60112PLC 1
Surface resistivityIEC 60093>1.0E+16ohms
hardnessTest ConditionTest MethodTest ResultTest Unit
Rockwell hardnessL-SaleISO 2039-2123
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.