PP Galloo GP-PP-157 Galloo Plastics S.A.
0
Technical Data Sheet
| impact performance | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Impact strength of cantilever beam gap | 23°C | ISO 180 | >7.0 kJ/m² |
| mechanical properties | Test Condition | Test Method | Test Result |
|---|---|---|---|
| tensile strength | Yield | ISO 527-2 | >20.0 MPa |
| Break | ISO 527-2 | >13.0 MPa | |
| Tensile strain | Break | ISO 527-2 | >30 % |
| Bending modulus | ISO 178 | 950 MPa |
| thermal performance | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Hot deformation temperature | 1.8MPa,Unannealed | ISO 75-2/A | >48.0 °C |
| Vicat softening temperature | ISO 306/A | >120 °C |
| Physical properties | Test Condition | Test Method | Test Result |
|---|---|---|---|
| density | Internal Method | 0.880to0.920 g/cm³ | |
| melt mass-flow rate | 230°C/2.16kg | ISO 1133 | 13to17 g/10min |
| hardness | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Shore hardness | ShoreD | ISO 868 | >62 |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.