Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|
density | | ISO1183 | 1.30 g/cm³ |
melt mass-flow rate | | ISO1133 | 3.0 g/10min |
Shrinkage rate | | STM640808 | 1.4 % |
Shrinkage rate | | STM640808 | 0.50 % |
water content | | ISO960 | 0.15 % |
flammability | Test Condition | Test Method | Test Result |
---|
Hot filament ignition temperature | | IEC60695-2-13 | 650 °C |
UL flame retardant rating | | UL94 | HB |
Mechanical properties | Test Condition | Test Method | Test Result |
---|
Tensile modulus | | ISO527-2 | 7400 MPa |
Tensile stress | Yield | ISO527-2 | 140 MPa |
Tensile strain | Yield | ISO527-2 | 3.0 % |
Flexural modulus | | ISO178 | 6300 MPa |
Bending stress | | ISO178 | 200 MPa |
Impact resistance | Test Condition | Test Method | Test Result |
---|
Charpy Notched Impact Strength | | ISO179 | 7.0 kJ/m² |
Charpy Notched Impact Strength | | ISO179 | 10 kJ/m² |
Impact strength of simply supported beam without notch | | ISO179 | 27 kJ/m² |
Impact strength of simply supported beam without notch | | ISO179 | 50 kJ/m² |
Thermal performance | Test Condition | Test Method | Test Result |
---|
| | ISO75-2/B | 200 °C |
vicat | | ISO306/B | 210 °C |
| | ISO3146 | 220 °C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.