TPU 58123 TPU Lubrizol Advanced Materials, Inc.
Typical Applications:
Wire and cable applications blown film cast film cable sheath
Product Description
Certificates(0)
Datasheet
Product Description
| Typical Applications: | Wire and cable applications | blown film | cast film | cable sheath |
Certificates
No Data...
Technical Data Sheet
| elastomer | Test Condition | Test Method | Test Result | Test Unit |
|---|---|---|---|---|
| elongation | Break | ASTM D412 | 730 | % |
| tensile strength | Break | ASTM D412 | 36.5 | MPa |
| tear strength | Split | ASTM D470 | 20 | kN/m |
| --5 | ASTM D624 | 66.7 | kN/m | |
| tensile strength | 300%Strain | ASTM D412 | 5.50 | MPa |
| 100%Strain | ASTM D412 | 3.40 | MPa | |
| Stretch permanent deformation | 200%Strain | ASTM D412 | 6 | % |
| mechanical properties | Test Condition | Test Method | Test Result | Test Unit |
| Taber abraser | 1000Cycles,1000g,H-18Wheel | ASTM D3389 | 17.0 | mg |
| thermal performance | Test Condition | Test Method | Test Result | Test Unit |
| Kofler Melting Temperature | Internal Method | 150 | °C | |
| Melting temperature | DSC | 135 | °C | |
| Glass transition temperature | ASTM D3418 | -70.0 | °C | |
| Physical properties | Test Condition | Test Method | Test Result | Test Unit |
| density | ASTM D792 | 1.06 | g/cm³ | |
| hardness | Test Condition | Test Method | Test Result | Test Unit |
| Shore hardness | ShoreA | ASTM D2240 | 70 | |
| film | Test Condition | Test Method | Test Result | Test Unit |
| Water vapor permeability | 38°C,Mocon法 | ASTM D6701 | 3200 | g/m²/24hr |
| ASTME96 | 420 | g/m²/24hr |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.