TPU 2780 NINGBO KINGSUI

52

Technical Data Sheet

processabilityTest ConditionTest MethodTest Result
Dry conditions80℃ 2-3小时
process temperature140-160 °C
process temperature175-185 °C
process temperature170-180 °C
process temperature180-190 °C
Temperature20-30 °C
pressure45-60 Mpa
Mechanical propertiesTest ConditionTest MethodTest Result
Tensile modulusASTM D412/ISO 5273.6 Mpa/Psi
Tensile modulusASTM D412/ISO 5277.5 Mpa/Psi
tensile strength ASTM D412/ISO 52736 Mpa/Psi
tear strengthASTM D624/ISO 3485 n/mm²
Shore hardnessASTM D2240/ISO 86880+-2 Shore A
ResilienceASTM D2630/ISO 466257 %
Physical propertiesTest ConditionTest MethodTest Result
densityASTM D792/ISO 2781/JIS K73111.18
Thermal performanceTest ConditionTest MethodTest Result
Glass Transition TemperatureASTM D3418/ISO 815-40 ℃(℉)
vicatASTM D1525/ISO R30680 ℃(℉)
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.