Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|
density | | ASTMD1505 | 0.940 g/cm³ |
melt mass-flow rate | | ASTMD1238 | 2.5 g/10min |
Vinyl acetate content | | | 18.5 wt% |
optical performance | Test Condition | Test Method | Test Result |
---|
gloss | | ASTMD2457 | 82 |
Haze ratio | | ASTMD1003 | 3.6 % |
Supplementary Information | Test Condition | Test Method | Test Result |
---|
BlownFilmMeltTemperature | | | <177 °C |
Cast Film Melt Temperature | | | <204 °C |
film | Test Condition | Test Method | Test Result |
---|
Tensile strain | | ASTMD882 | 800 % |
Falling hammer impact | | ASTMD1709 | 290 g |
Film thickness - tested | | | 32 µm |
Secant modulus | | ASTMD882 | 42.1 MPa |
Secant modulus | | ASTMD882 | 50.3 MPa |
tensile strength | | ASTMD638 | 24.8 MPa |
tensile strength | | ASTMD638 | 24.1 MPa |
Tensile strain MD | | ASTMD882 | 600 % |
Thermal performance | Test Condition | Test Method | Test Result |
---|
vicat | | ASTMD1525 | 67.0 °C |
| | ASTMD3418 | 85.0 °C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.