PP Copolymer Tecnoprene® 3K8EL9 NERO900 SO.F.TER ITALY
Properties:
Filler glass fiber reinforced material 40% filler by weight
Product Description
Certificates(0)
Datasheet
Product Description
| Properties: | Filler | glass fiber reinforced material | 40% | filler by weight |
Certificates
No Data...
Technical Data Sheet
| mechanical properties | Test Condition | Test Method | Test Result | Test Unit |
|---|---|---|---|---|
| tensile strength | 23°C | ASTM D638 | 70 | MPa |
| bending strength | 23°C | ASTM D790 | 110 | MPa |
| Bending modulus | 23°C | ASTM D790 | 6200 | MPa |
| Impact strength of cantilever beam gap | 23°C | ASTM D256 | 272 | J/m |
| thermal performance | Test Condition | Test Method | Test Result | Test Unit |
| Linear coefficient of thermal expansion | MD | ASTM D696 | 2.8E-05 | cm/cm/°C |
| Hot deformation temperature | 1.80MPaUnannealed | ASTM D648 | 145 | °C |
| Physical properties | Test Condition | Test Method | Test Result | Test Unit |
| density | ASTM D792 | 1.21 | g/cm³ | |
| Shrinkage rate | MD | ASTM D995 | 0.30 | % |
| Water absorption rate | (23°C,24hr) | ASTM D570 | 0.020 | % |
| melt mass-flow rate | 230℃/2.16Kg | ASTM D1238 | 3.5 | g/10min |
| 灰分 | Internal Method | 40 | % | |
| Electrical performance | Test Condition | Test Method | Test Result | Test Unit |
| Dissipation factor | 相对漏电起痕指数 | ASTM D3638 | 650 | V |
| Surface resistivity | ASTM D257 | 1E+15 | Ω.cm | |
| Dielectric constant | ASTM D150 | 2.50 | 1kHz | |
| flame retardant performance | Test Condition | Test Method | Test Result | Test Unit |
| UL flame retardant rating | UL -94 | HB | 3.20mm |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.