thermosetting | Test Condition | Test Method | Test Result |
---|
| | | 按重量计算的混合比:100 |
| | | 按重量计算的混合比:120 |
physical property | Test Condition | Test Method | Test Result |
---|
Water absorption rate- | | 内部方法 | 0.10 % |
density | | ASTMD792,ASTMD1622 | 1.25 g/cm³ |
Shrinkage rate | | 内部方法 | 0.43 % |
Supplementary Information | Test Condition | Test Method | Test Result |
---|
DartImpact | | 内部方法 | 801 J/m |
HeatSag | | ASTMD3769 | 3.60 mm |
HeatSag | | ASTMD3769 | 0.500 mm |
Mechanical properties | Test Condition | Test Method | Test Result |
---|
Flexural modulus | | ASTMD790 | 1100 MPa |
tensile strength | | ASTMD638 | 37.9 MPa |
elongation | | ASTMD638 | 40 % |
Flexural modulus | | ASTMD790 | 2760 MPa |
Flexural modulus | | ASTMD790 | 1720 MPa |
elastomer | Test Condition | Test Method | Test Result |
---|
tensile strength | | ASTMD412 | 37.9 MPa |
elongation | | ASTMD412 | 40 % |
tear strength | | ASTMD624 | 97.2 kN/m |
Thermal performance | Test Condition | Test Method | Test Result |
---|
| | ASTMD696 | 3.8E-05 cm/cm/°C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.