HDPE DMDA-6200 Natural 7 DOW USA
60
Form:Granules
Properties:
High melt strengthResistance to stress cracHigh impact resistanceExcellent resistance to eHigh melting pointHigh impact resistance e
Typical Applications:
Household appliancesThin walled componentschipUsed for household industrial chemicals
Product Description
Certificates(0)
Datasheet
Product Description
| Typical Applications: | Household appliances | Thin walled components | chip | Used for household industrial chemicals |
| Properties: | High melt strength | Resistance to stress crac | High impact resistance | Excellent resistance to e | High melting point | High impact resistance | e |
Certificates
No Data...
Technical Data Sheet
| Basic Performance | Test Condition | Test Method | Test Result | Test Unit |
|---|---|---|---|---|
| melt mass-flow rate | 190℃/2.16kg | ASTM D-1238 | 0.38 | g/10min |
| 190℃/21.6kg | ASTM D-1238 | 33 | g/10min | |
| density | ASTM D-792 | 0.953 | ||
| mechanical properties | Test Condition | Test Method | Test Result | Test Unit |
| Bending modulus | 2%割线 | ASTM D-790 B | 145.000(1000) | Psi(MPa) |
| Environmental stress cracking resistance | 122 | ASTM D-1693 | 80 | hrs |
| tensile strength | Break | ASTM D-638 | 4500(31) | Psi(MPa) |
| Impact strength of cantilever beam gap | ASTM D-1822 | 80(168) | ft·lb/in2(kJ/m2) | |
| Shore hardness | ASTM D-2240 | 61 | Shore D | |
| elongation | Break | ASTM D-638 | 1000 | % |
| elongation at yield | ASTM D-638 | 7 | % | |
| tensile strength | Yield | ASTM D-638 | 3900(27) | Psi(MPa) |
| thermal performance | Test Condition | Test Method | Test Result | Test Unit |
| Vicat softening temperature | ASTM D-1525 | 264(129) | ||
| Hot deformation temperature | 66psi(0.45MPa) | ASTM D-648 | 163(73) | |
| Crystallization peak temperature | DSC法 | Dow Method | 244(118) | |
| Melting temperature | DSC法 | Dow Method | 268(131) |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.