PBT 3316 JAPAN POLYPLASTIC
129
Form:Granules | Grade:Enhanced level
Properties:
Glass fiber reinforced
Typical Applications:
Fitness equipmentCasters
Product Description
Certificates(0)
Datasheet
Product Description
| Typical Applications: | Fitness equipment | Casters |
| Properties: | Glass fiber reinforced |
Certificates
No Data...
Technical Data Sheet
| other | Test Condition | Test Method | Test Result | Test Unit |
|---|---|---|---|---|
| characteristic | GF30% | |||
| Other performance | Test Condition | Test Method | Test Result | Test Unit |
| Surface resistivity | --- | --- | 1×1016 | Ω |
| Arc resistance | *2 | --- | 250 | V |
| *2 | --- | 92 | S | |
| Basic Performance | Test Condition | Test Method | Test Result | Test Unit |
| density | --- | ASTM D-792 | 1.66 | --- |
| mechanical properties | Test Condition | Test Method | Test Result | Test Unit |
| Charpy Notched Impact Strength | ASTM D256/ISO 179 | 98 | kg·cm/cm(J/M)ft·lb/in | |
| Elongation at Break | ASTM D638/ISO 527 | 2.7 | % | |
| tensile strength | ASTM D638/ISO 527 | 147 | kg/cm²(MPa)[Lb/in²] | |
| Bending modulus | ASTM D790/ISO 178 | 9610 | kg/cm²(MPa)[Lb/in²] | |
| bending strength | ASTM D790/ISO 178 | 225 | kg/cm²(MPa)[Lb/in²] | |
| tensile strength | --- | ASTM D-638 | 147 | Mpa |
| Bending modulus | --- | ASTM D-790 | 9610 | Mpa |
| Elongation at Break | --- | ASTM D-638 | 2.7 | % |
| bending strength | --- | ASTM D-790 | 225 | Mpa |
| Impact strength of cantilever beam gap | Notched,--- | ASTM D-256 | 98 | J/m |
| 反Notched侧,--- | ASTM D-256 | 680 | J/m | |
| thermal performance | Test Condition | Test Method | Test Result | Test Unit |
| Combustibility (rate) | UL 94 | V-0 | ||
| Hot deformation temperature | HDT | ASTM D648/ISO 75 | 212 | ℃(℉) |
| Linear coefficient of thermal expansion | ASTM D696/ISO 11359 | 2-7 | mm/mm.℃ | |
| 室温 | --- | 2-7 | ×10-5/℃ | |
| UL flame retardant rating | --- | UL 94 | V-0 | --- |
| Hot deformation temperature | 1.82MPa | ASTM D-648 | 212 | °C |
| Physical properties | Test Condition | Test Method | Test Result | Test Unit |
| density | ASTM D792/ISO 1183 | 1.66 | ||
| Electrical performance | Test Condition | Test Method | Test Result | Test Unit |
| Surface resistivity | ASTM D257/IEC 60093 | 1×10^16 | Ω | |
| Volume resistivity | ASTM D257/IEC 60093 | 1×10^16 | Ω.cm | |
| 3mmt | ASTM D-257 | 1×1016 | Ω.cm | |
| Dielectric strength | 短时:3mmt | ASTM D-149 | 20 | MV/m |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.