Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|
Crystallinity | | ASTMD3417 | 48 % |
Crystallinity | | ASTMD3417 | 47 % |
Crystallinity | | ASTMD3417 | 50 % |
relative viscosity | | ASTMD4020 | 230到350 cm³/g |
relative viscosity | | ASTMD4020 | 230到350 cm³/g |
relative viscosity | | ASTMD4020 | 230到350 cm³/g |
density | | ASTMD792 | 0.930 g/cm³ |
hardness | Test Condition | Test Method | Test Result |
---|
| | ASTMD2240 | 65 |
| | ASTMD2240 | 65 |
| | ASTMD2240 | 65 |
Mechanical properties | Test Condition | Test Method | Test Result |
---|
Tensile modulus | | ASTMD638 | 731 MPa |
Tensile modulus | | ASTMD638 | 672 MPa |
tensile strength | | ASTMD638 | 23.0 MPa |
tensile strength | | ASTMD638 | 20.0 MPa |
tensile strength | | ASTMD638 | 22.0 MPa |
tensile strength | | ASTMD638 | 53.0 MPa |
tensile strength | | ASTMD638 | 49.0 MPa |
tensile strength | | ASTMD638 | 44.0 MPa |
elongation | | ASTMD638 | 60 % |
Tensile modulus | | ASTMD638 | 725 MPa |
elongation | | ASTMD638 | 470 % |
| | ASTMD1894 | 0.10到0.22 |
| | ASTMD1894 | 0.050到0.10 |
| | ASTMD1894 | 0.050到0.080 |
| | ASTMD1894 | 0.14 |
| | ASTMD1894 | 0.13 |
| | ASTMD1894 | 0.14 |
| | ASTMD1894 | 0.16 |
| | ASTMD1894 | 0.16 |
| | ASTMD1894 | 0.16 |
elongation | | ASTMD638 | 460 % |
Impact resistance | Test Condition | Test Method | Test Result |
---|
Impact strength of cantilever beam gap | | ASTMD256 | 80 J/m |
Electrical performance | Test Condition | Test Method | Test Result |
---|
Volume resistivity | | ASTMD257 | >2.0E+7 ohms·cm |
dielectric strength | | ASTMD149 | 14 kV/mm |
dielectric constant | | ASTMD150 | 2.48 |
dielectric constant | | ASTMD150 | 2.45 |
dielectric constant | | ASTMD150 | 2.54 |
Dissipation Factor | | ASTMD150 | 0.059 |
Dissipation Factor | | ASTMD150 | 0.11 |
Surface Resistivity | | ASTMD257 | 1E+03 ohms |
Surface Resistivity | | ASTMD257 | 1E+03 ohms |
Surface Resistivity | | ASTMD257 | 1E+03 ohms |
Volume resistivity | | ASTMD257 | 6E+07 ohms·cm |
Volume resistivity | | ASTMD257 | 1.5E+07 ohms·cm |
Dissipation Factor | | ASTMD150 | 0.23 |
Dissipation Factor | | ASTMD150 | 8.2E-03 |
Dissipation Factor | | ASTMD150 | 2.2E-03 |
Dissipation Factor | | ASTMD150 | 3.4E-03 |
Dissipation Factor | | ASTMD150 | 0.10 |
Dissipation Factor | | ASTMD150 | 0.021 |
Dissipation Factor | | ASTMD150 | 0.069 |
Thermal performance | Test Condition | Test Method | Test Result |
---|
| | | 134 °C |
| | | 136 °C |
| | ASTMD696 | 9.2E-04 cm/cm/°C |
| | ASTMD696 | 1.5E-04 cm/cm/°C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.