Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|
Specific volume | | ASTMD792 | 0.835 cm³/g |
melt mass-flow rate | | ASTMD1238 | 18 g/10min |
Shrinkage rate | | 内部方法 | 0.50to0.70 % |
Water absorption rate | | ASTMD570 | 0.15 % |
Water absorption rate | | ASTMD570 | 0.35 % |
Water absorption rate | | ASTMD570 | 0.58 % |
Outdoor applicability | | UL746C | f1 |
hardness | Test Condition | Test Method | Test Result |
---|
Rockwell hardness | | ASTMD785 | 70 |
Rockwell hardness | | ASTMD785 | 118 |
optical performance | Test Condition | Test Method | Test Result |
---|
refractive index | | ASTMD542 | 1.586 |
transmissivity | | ASTMD1003 | 88.0 % |
Haze ratio | | ASTMD1003 | 1.0 % |
flammability | Test Condition | Test Method | Test Result |
---|
UL flame retardant rating | | UL94 | HB |
Mechanical properties | Test Condition | Test Method | Test Result |
---|
elongation | | ASTMD638 | 110 % |
Flexural modulus | | ASTMD790 | 2340 Mpa |
bending strength | | ASTMD790 | 93.1 Mpa |
| | ASTMD1044 | 10.0 mg |
tensile strength | | ASTMD638 | 62.1 Mpa |
tensile strength | | ASTMD638 | 65.5 Mpa |
elongation | | ASTMD638 | 7.0 % |
Impact resistance | Test Condition | Test Method | Test Result |
---|
Falling hammer impact | | ASTMD3029 | 169 J |
Tensile impact strength 4 | | ASTMD1822 | 546 kJ/m² |
Electrical performance | Test Condition | Test Method | Test Result |
---|
Volume resistivity | | ASTMD257 | >1.0E+17 ohms·cm |
dielectric strength | | ASTMD149 | 15 KV/mm |
dielectric constant | | ASTMD150 | 3.17 |
dielectric constant | | ASTMD150 | 3.17 |
dielectric constant | | ASTMD150 | 2.96 |
Dissipation Factor | | ASTMD150 | 9E-04 |
Dissipation Factor | | ASTMD150 | 9E-04 |
Dissipation Factor | | ASTMD150 | 0.010 |
Compared to the Leakage Tracking Index (CTI) | | UL746 | PLC 2 |
High arc combustion index (HAI) | | UL746 | PLC 1 |
High Voltage Arc Traceability Rate (HVTR) | | UL746 | PLC 2 |
Hot wire ignition (HWI) | | UL746 | PLC 4 |
Thermal performance | Test Condition | Test Method | Test Result |
---|
| | ASTMD648 | 138 °C |
| | ASTMD648 | 132 °C |
vicat | | ASTMD15255 | 154 °C |
| | ASTME831 | 6.8E-05 cm/cm/°C |
specific heat | | ASTMC351 | 1260 J/kg/°C |
thermal conductivity | | ASTMC177 | 0.19 W/m/K |
RTI Elec | | UL746 | 130 °C |
RTI Imp | | UL746 | 130 °C |
RTI Str | | UL746 | 130 °C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.